Hi all,

I am testing a capacitive accelerometer. I found the initial capacitance from
chip level testing (~20 pF) was far larger than the one from wafer level testing
(~10 pF). Both the chip level and wafer level testing was done with the same
probe on the same probe station. This phenomenon happened on all chips. Could
anyone tell me why there is so large parasitic capacitance during chip level
testing? Thanks.

Best Regards,

Jin
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
University Wafer
Addison Engineering
Tanner EDA by Mentor Graphics