PDMS mold peeling off process
2011-03-17
첸로
2011-03-17
righeira carnegie
2011-03-17
Xiaohui Lin
2011-03-17
Mikael Evander
2011-03-18
righeira carnegie
2011-03-22
Tsoll Doiiu
2011-03-22
[email protected]
2011-03-17
Barbara Cortese
PDMS mold peeling off process
[email protected]
2011-03-22
Hi,

Check very carefully your humidity and temperature from your cleanroom
where you prepare the master. Look to the validity date of the resist that
you are using.

How long you bake the PDMS?

On Mar 17, 2011 4:57am, "첸로"  wrote:

> Dear all,
>
> I am using photolithography and PDMS mold technique to get a PDMS mold.
> I'm having some troubles when I peel off the PDMS mold from the SU-8
> master. Even a very careful handing I can not get a good PDMS mold. After
> peeling off, the pattern on the PDMS mold is always broken.
> The SU-8 master's smallest width is 10um. Is it feasible in theory?
>
> Can anyone give me some suggestions?
>
> Thank you in advance
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Mentor Graphics Corporation