MEMSnet Home: MEMS-Talk: Re: Pyrex 7740
Re: Pyrex 7740
1999-05-24
Philip Floyd
Re: Pyrex 7740
Philip Floyd
1999-05-24
You can try:

Swift Glass Co.
P.O.  Box 879
Elmira, NY 14092
(607)733-7166  Voice
(607) 732-5829 FAX

Phil



At 08:53 PM 5/20/99 PDT, Wiranto, Goib - WIRGY001 wrote:
>Dear all,
>
>I'm looking for 50 pcs of 1 mm thick, 2 by 2 inch, single side polished Pyrex
>glass for
>anodic bonding with silicon.
>
>If anyone can give me names and addresses of companies or suppliers for such
>material
>will be very much appreciated.
>
>Thank you very much.
>
>Goib Wiranto
>Microelectronics Centre
>University of South Australia
>Mawson Lakes, SA 5095
>Australia
>email: [email protected]
>
>
>
***********************************
Philip D. Floyd, Ph.D.
Member of the Research Staff
Electronic Materials Laboratory
Xerox Palo Alto Research Center
3333 Coyote Hill Rd., 35-1170
Palo Alto, CA 94304
Voice: 650-812-4129
FAX:   650-812-4105
E-mail:[email protected]
***********************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
MEMS Technology Review
Process Variations in Microsystems Manufacturing