A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RIE Etching SiO2/Si
RIE Etching SiO2/Si
2011-06-06
Judith Linacero Blanco
2011-06-06
Khaled Mohamed Ramadan
2011-06-07
Glenn Silveira
2011-06-06
Andrew Sarangan
2011-06-06
Gary Hillman
2011-06-09
Judith Linacero Blanco
2011-06-09
Judith Linacero Blanco
2011-06-09
Robert Ditizio
2011-06-07
antwi nimo
2011-06-07
SALVADOR_ALCANTARA_INIESTA
RIE Etching SiO2/Si
SALVADOR_ALCANTARA_INIESTA
2011-06-07
  Hi,

Other posibility is with wet etching. KOH to 30% in weigth in H2O solution,
to 70 or 80°C.

                 SAI

antwi nimo escribió:

> You want to etch silicon with selectivity to oxide.  RIE is good as you have
done.
>
> You just have to play with the gases.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
Nano-Master, Inc.