Contact-free cleaning of limestone on FS/Ta2O5 substrates
2011-06-12
Martin Rumpel
2011-06-13
Ruiz, Marcos Daniel (SENCOE)
2011-06-14
Roger Shile
Contact-free cleaning of limestone on FS/Ta2O5 substrates
Roger Shile
2011-06-14
My experience with extremely hard well water is vinegar to remove
residue from coffee maker and cooking utensils, muriatic acid to clean
toilet bowels ...

Roger Shile

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
Ruiz, Marcos Daniel (SENCOE)
Sent: Monday, June 13, 2011 10:13 AM
To: General MEMS discussion; [email protected]
Subject: [mems-talk] Contact-free cleaning of limestone on
FS/Ta2O5substrates

Unfortunately, dried liquid residue (water spots) is notoriously
difficult to remove.  I would recommend Summa Clean (basically a soapy
mixture) and agitation in a megasonic or ultrasonic tank - as aggressive
as your samples can handle.

Dan Ruiz

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review