A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Ti etching and S1813 resist
Ti etching and S1813 resist
2011-07-12
Shane GUO
2011-07-12
Kirt Williams
2011-07-12
Michael Martin
2011-07-12
Shane GUO
2011-07-12
G. Puebla-Hellmann
2011-07-13
David Springer
2011-07-17
Yunda Wang
2011-07-14
Shane GUO
Ti etching and S1813 resist
Kirt Williams
2011-07-12
Ion milling with argon will work for only 0.1 um of Ti.

   --Kirt Williams

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf
Of Shane GUO
Sent: Tuesday, July 12, 2011 8:57 AM
To: [email protected]
Subject: [mems-talk] Ti etching and S1813 resist

Hi all,

I would like to use S1813 resist as an etching mask for Ti. I am wondering
if there is anything that does not contain HF can work for me? I am thinking
about oxalic acid or H2O2. Do they attack S1813 resist? Can they work for a
100nm Ti layer? Any suggestion is welcome.


Best regards
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Mentor Graphics Corporation