Recommend a negative resist
2011-08-05
Ned Flanders
2011-08-05
Kevin Nichols
2011-08-06
Ned Flanders
2011-08-06
Bill Moffat
2011-08-06
Kevin Nichols
2011-08-07
Ned Flanders
2011-08-06
Xiaohui Lin
2011-08-05
gau s
2011-08-05
gau s
Recommend a negative resist
Bill Moffat
2011-08-06
Ned tell us more of what you want to do.  For example with positive resist and
metal lift off you can do repeatable 0.1 micron dimensions.  Bill Moffat

________________________________________
From: [email protected] [mems-talk-
[email protected]] on behalf of Ned Flanders
[[email protected]]
Sent: Saturday, August 06, 2011 1:18 AM
To: Kevin Nichols
Cc: General MEMS discussion
Subject: Re: [mems-talk] Recommend a negative resist

Thanks, but I need something that I can easily strip. That excludes SU-8.

As for how thick: well, since I need 1 um resolution or better, it
should be thinner than 1 um.

m
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMStaff Inc.