A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Pin holes in thermal oxide
Pin holes in thermal oxide
2012-01-22
H V Balachandra Achar
2012-01-23
Felix Lu
2012-01-23
Gary Hillman
2012-01-23
Shay
2012-01-23
Morrison, Richard H., Jr.
2012-01-23
Matthieu Nannini, Dr.
Pin holes in thermal oxide
Morrison, Richard H., Jr.
2012-01-23
Hi,

Your pre-oxide clean is incorrect, use Sulfuric/H2O2 at 130c for 20
minutes, get the sulfuric to 130c then add 100ml of H2O2 slowly.
followed by SC1, SC2 and 50:1 HF dip, that will give you a clean
surface.

If the wafers are new out of the box you can skip the clean, nothing is
better than clean wafers right out of the box.

Rick


Rick Morrison
Senior Member Technical  Staff
Group Leader Microfabrication Operations
Draper Laboratory
555 Technology Square
Cambridge, MA  02139

W  617-258-3420
C   508-930-3461



-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of
H V Balachandra Achar
Sent: Sunday, January 22, 2012 3:03 AM
To: [email protected]
Subject: [mems-talk] Pin holes in thermal oxide

Dear All,

I am using 1 micron thick thermal oxide, grown using dry-wet-dry
sequence, as
the mask during bulk etching of silicon using KOH solution. After
oxidation I
notice pin holes in oxide surface. Because of these pin holes, silicon
is
getting etched in KOH at places where I don't want to etch.

Please suggest a remedy.

Note: I am using (100) p-type 1-10 ohm-cm Si wafer.
Cleaning sequence: TCE, acetone, nitric acid, dilute HF
Dry-wet-dry durations: 20 min - 4 hrs - 20 min, followed by 30 min
annealing
in N2 ambient.

Thank you

--
H V Balachandra Achar

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing