MEMSnet Home: MEMS-Talk: Magic liquid etchant: etches alumina faster than aluminum?
Magic liquid etchant: etches alumina faster than aluminum?
2012-06-20
Ned Flanders
2012-06-20
Kevin Nichols
2012-06-27
Ned Flanders
Magic liquid etchant: etches alumina faster than aluminum?
Ned Flanders
2012-06-20
Does it exist?
If it etches alumina and not aluminum at all, it gets extra magic points.


Help?
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review