Dear MEMS researchers:
I research detailed informations about the deposition of optical
polymers such as polyimides, siloxane, PMMA, and other (but having
optical properties). The application is the fabrication of low-loss
optical waveguides, combined with standard MEMS technology. Also, the
deposition process must to be compatible with MEMS micromachining (low
temperature processing). If the patterning of these waveguides is well
described in the literature (NTT, Du Pont), the deposition chemistry
process is not easily available. Usually, this process is closed to the
sol-gel but modified (reflow bellow 300°C).
If you have some information sources (publications, web, etc.) please
send me it.
Also, I am looking for mechanical parameters of polymers (Young,
Poisson, etc.)
Sincerely yours,
C. Gorecki

*******************************************************************
Dr. Christophe Gorecki, Senior Researcher
Laboratoire d'Optique P.M. Duffieux,Université de Franche-Comté
16 Rte de Gray, 25030 Besançon Cedex, France
Tel: +33-3-81666594, fax: 33-3-81666423
e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer