MEMSnet Home: MEMS-Talk: Reflected platen power problem in STS ICP615 - RIE machine
Reflected platen power problem in STS ICP615 - RIE machine
2015-04-12
Serdar Taze
Reflected platen power problem in STS ICP615 - RIE machine
Serdar Taze
2015-04-12
Dear distinguished members of mems-talk,
I am trying to microfabricate micro grooves which are 200um x200um lines
and spaces in term of lithography mask.
I am using STS ICP615 - RIE machine, and a Bosch process with SF6 and O2
for Si etch, and C4F8 for surface polymerization. I tried many recipes,
and finally found a suitable one. Recently, I realized that the determined
recipe is no longer working. From tool log files I found out that, for
some reason the reflected platen power is larger compared to previous
recipe runs. The platen power that is used in the processes, was 13W in
13.56MHz platen. In earlier processes, the reflected power was almost 0 W.
However, right now, reflected platen power is measured as 7-8 W. I tried
to clean the chamber with O2 for 30min hoping that cleaning the chamber
may help with reducing the reflected platen power. I applied the same
recipe and found that the resultant reflected power is still around 7-8 W.
Soon, I will try longer O2 cleaning time. But I am not sure if that will
solve my problem.
If you faced this problem before and know what would solve the problem, or
if you have an idea on how to solve it, could you please share your
knowledge as soon as possible?
Thanks in advance,

Regards
Serdar Taze,
Student, M.Sc
Bilkent University Mechanical Engineering Program
Bilkent Üniversitesi, 06800 Bilkent, Ankara, Turkey
E-mail: [email protected], [email protected]


_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics