MEMSnet Home: MEMS-Talk: Re: Si-Nitride
Re: Si-Nitride
1999-07-15
lin wang
Re: Si-Nitride
lin wang
1999-07-15
Marc,

I don't noctice anything happened to the 1um thick nitride film after
10plus hour KOH etching the through holes. Just usual acetone or AHP clean
is fine. Good luck,

Lin