A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: How to make a metal grid
How to make a metal grid
2016-07-05
John Bohland
2016-07-06
Bill Moffat
2016-07-06
Bill Moffat
2016-07-06
Gary Hillman
2016-07-06
[email protected]
2016-07-07
Philipp Altpeter
2016-07-07
Wilson, Thomas
2016-07-07
Andrew Sarangan
2016-07-12
Daniel Figura
2016-07-12
Roberto Igal Chertkow
2016-07-13
John Bohland
How to make a metal grid
[email protected]
2016-07-06
Al Dry etch or if you dont have it, lift -off maybe

----- Original Message -----
From: John Bohland 
Date: Wednesday, July 6, 2016 1:19
Subject: [mems-talk] How to make a metal grid
To: "[email protected]" 

> I am interested in making a metal grid on a 370 mm X 470 mm
> glass substrate.
>
> The problem is that the metallization lines must be only 1.5
> microns in width and spaced (pitch) only a few microns apart.
>
> The metal can be Al or Ag and 100 nm thick.
>
> The best idea I have is to monolithically coat the glass with
> sputtered (PVD) Al or Ag then use a picoseond laser to remove
> all but the desired 1.5 micron wide metal line widths. Even then
> I don't know if the laser would have good enough resolution to
> meet these requirements.
>
> Anyone have better ideas?
>
> Thanks,
>
> John
>
> NOTICE
> This transmittal and/or attachments ("Communication") is
> confidential to Bloo Solar, or may otherwise be privileged
> information. If you are not the intended recipient, you are
> hereby notified that you have received this Communication in
> error and any dissemination, distribution or copying of this
> Communication is strictly prohibited. If you have received this
> Communication in error, please notify us immediately and
> promptly delete and purge this Communication.
>
> _______________________________________________
> Hosted by the MEMS and Nanotechnology Exchange, the country's leading
> provider of MEMS and Nanotechnology design and fabrication services.
> Visit us at http://www.mems-exchange.org
>
> Want to advertise to this community?  See http://www.memsnet.org
>
> To unsubscribe:
> http://mail.mems-exchange.org/mailman/listinfo/mems-talk
_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing