A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Would you help me to solve one problem
Would you help me to solve one problem
1999-07-22
Jorge Felipe
Would you help me to solve one problem
Jorge Felipe
1999-07-22
This is a multi-part message in MIME format.

------=_NextPart_000_0004_01BED3DD.5F508C20
Content-Type: text/plain;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable

I need to make gold alloy by using silicon metal to reduce the melt =
temperature and to make the metal become fluid to make micro casting.
I need to use silicone to make the gold deoxiding, to avoid porosity the =
pieces casting.
I am making alloy :22% of pure silver and 10.3% of pure copper .
How much % of silicon metal, I need to add to make a good deoxidizing ?
Would you help me to solve this problem
My E-mail is :[email protected]

------=_NextPart_000_0004_01BED3DD.5F508C20
Content-Type: text/html;
        charset="iso-8859-1"
Content-Transfer-Encoding: quoted-printable









I need to make gold alloy by using = silicon metal=20 to reduce the melt temperature and to make the metal become fluid to = make micro=20 casting.
I need to use silicone to make the = gold=20 deoxiding, to avoid porosity the pieces casting.
I am making alloy :22% of pure = silver and 10.3%=20 of pure copper .
How much % of silicon metal, I need = to add to=20 make a good deoxidizing ?
Would you help me to solve this=20 problem
My E-mail is=20 :[email protected]
------=_NextPart_000_0004_01BED3DD.5F508C20--
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMStaff Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing