MEMSnet Home: MEMS-Talk: Wet etchant for TiN films
Wet etchant for TiN films
1999-07-28
[email protected]
Wet etchant for TiN films
[email protected]
1999-07-28
What is a typical wet etch for TiN films?

Sincerely,
Thomas A Deis

*  Voice: (517) 496-6719
*   Fax:  (517) 496-5121
*  Mail:  C041D1 (DC-4)
* e-mail: [email protected]

***********************************************************
This email transmission and any files that accompany it may
contain sensitive information belonging to the sender. The
information is intended only for the use of the individual
or entity named. If you are not the intended recipient, you
are hereby notified that any disclosure, copying,
distribution, or the taking of any action in reliance on the
contents of this information is strictly prohibited. If you
have received this email transmission in error, please
immediately notify the Security Administrator.
[email protected]
***********************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMS Technology Review
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing