[email protected]
chromium lift-off from pyrex glass, etch
[email protected]
1999-02-02
Have you considered dry etching?  It is possible to achieve high aspect
ratio holes using RIE or ICP techniques.  Your sputtered chrome would be a
suitable mask.  How deep do you want to go?

Martin Walker
***********************************************
Plasma Technology, Oxford Instruments
North End, Yatton
Bristol, BS49 4AP, England
Tel: +44 (0)1934 833851 Fax: +44 (0)1934 834918
URL http://www.oxfordplasma.com/
***********************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Addison Engineering
Harrick Plasma, Inc.