MEMSnet Home: MEMS-Talk: Re: Obtaining Polyimides/Vias in Polyimides
Re: Obtaining Polyimides/Vias in Polyimides
1999-02-03
Zhimin Jamie Yao
Re: Obtaining Polyimides/Vias in Polyimides
Zhimin Jamie Yao
1999-02-03
Avinash,

The following companies have many different kinds of polyimide.

OCG Microelectronic Materials Incorporated, 401-438-7805

Dow Chemical Company, and

HD MicroSystems, 1-800-346-5656, or Joe Butera:610-869-0834

Good Luck,

Jamie Yao

At 09:11 AM 1/28/99 -0800, you wrote:
>     Hello,
>
>     I need some information on how to obtain spin-on polyimides
>     (vendors, manufacturers, etc). I am looking to deposit
>     5-15 micron thick films.
>
>     Also, does anyone have any experience with via formation in
>     polyimides using the laser ablation technique. I need to
>     fabricate vias with tapered sidewalls (i.e., top via pad
>     is larger than bottom via pad)...
>
>     Thanks for your help,
>
>     Avinash Kane
>     Raytheon Systems Company
>     [email protected]
>
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
MEMS Technology Review
Tanner EDA by Mentor Graphics