Mac McReynolds
1999-02-19
Try Olin Microelectronic Materials
200 Massasoit Ave
East Providence, RI 02914
USA
Tel:  401-431-5388
Fax:  401-438-8018
*********************************************************
Mac McReynolds
Sr. R&D Process Engineer
Caliper Technologies
email:  [email protected]
www.calipertech.com

> ----------
> From:         Xu Guolin
> Reply To:     Xu Guolin;[email protected]
> Sent:         Friday, February 19, 1999 5:13 AM
> To:   [email protected]
> Subject:      Photo Polyamide
>
> Dear All,
>
>       Can anyone tell me where can I get photo polyamide ?
>
>       Thank you.
>
>       Guo Lin XU
>
> Xu Guolin
> ................................................................
> Manufacturing Division
> Dept. of Mech.& Prod. Eng.
> National University of Singapore
> 10 Kent Ridge Crescent
> Singapore 119260
> E-mail: [email protected]
> ...................................................................
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation