I have done some work using parylene as an anti-stiction agent.  In order to
probe through the coating I have to use very thin (75A) coatings which are not
adequately reproducible.

Does anyone have experience with selectively removing parylene?

Sincerely,
Maurice Karpman
Senior Engineer
Analog Devices, Inc
21 Osborn St
Cambridge, MA 02139
617-761-7201
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation