A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Re: SiO2 Wet etch rate?
Re: SiO2 Wet etch rate?
1999-03-15
Kirthi Roberts
1999-03-15
Amit Shiwalkar
1999-03-16
Andrezej Prochaska
Re: SiO2 Wet etch rate?
Kirthi Roberts
1999-03-15
park chang min wrote:
>
> Hello, mems.
> I want to know  etch rate of SiO2 etch rate using etchant Buffered HF (
> 6:1).(BOE)
> And I want to know that the etch rate of SiO2 using etchant KOH(20:80)
> H2O, too.
> Please let me know as soon as possible.
> Sincerely yours.
>
>
Hello,

With BOE the etch rate of SiO2 is about 1
micron/minute.

Kirthi

--
__________________________________
Kirthi Roberts
School of Engineering Science
Simon Fraser University
Vancouver
Canada
__________________________________
e-mail : [email protected]
URL: http://www.sfu.ca/~kroberts
__________________________________


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Addison Engineering
MEMS Technology Review