MEMSnet Home: MEMS-Talk: Re: photoresist spinner
Re: photoresist spinner
1999-04-15
Kevin M Walsh
1999-04-15
jneogi
1999-04-15
Klaus Ruhmer at Home
1999-04-15
Jim Beall
1999-04-15
[email protected]
1999-04-16
Shile
Re: photoresist spinner
Jim Beall
1999-04-15
>Our photoresist spinner died last week and we are looking for a new one.
>I found several manufacturers of small benchtop spinners - Headway,
>Laurell, Cost Effective Equipment (part of Brewer Science) and SCS
>(Specialty Coating System). Does anyone have experience, good or bad,
>with these spinners? Are there others that I should be looking into?

Winston -

We have bought about 10 Headway spinners over the past 15 years. They seem
like pretty good machines. The main failure mode is too much
acetone/photoresist being sucked down the vacuum line which ruins the motor
bearings after a few years. Motor replacement is about $1K.

We had one of the Laurell plastic machines (the very low end one) for a
dedicated HF process - it seemed fine for that and general wafer drying,
but I don't think that model had motor speed control. I know they make
speed copntrolled models also.

We also have a Solitec spin coater/developer setup which uses an offset
motor and belt drive arrangement for bearing protection. We don't have
enough experience with it yet to predict its lifetime.

good luck with your search,

Jim



 - Jim Beall 303-497-5989
   [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
MEMS Technology Review