MEMSnet Home: MEMS-Talk: Re: Piezoelectric materials
Re: Piezoelectric materials
1999-05-12
nigel r. sharma
1999-05-13
Joel Dubow
1999-05-13
Fahrettin Levent Degertekin
Re: Piezoelectric materials
Fahrettin Levent Degertekin
1999-05-13
Standard PZT-5H should satisfy your dielectric constant requirement.  You
can buy it from Vernitron Inc.

Levent

> > Hi!
> >
> > I am looking for a piezoelectric materials supplier.  I am interested on
> > a piezoelectric disk with a diameter of 1-2 cm, 1-5 mm thick, and
> > dielectric constant of the order of 1700. In practice, for our
> > applications don't care the electrode material.
> >
> > Can someone please help?
> >
> > Thanks in advance
> >
> > Dr. F. Sandoval-Ibarra
> >
> >
>
>
>

***********************************
F. Levent Degertekin
E.L. Ginzton Laboratory
Stanford University
Stanford, CA 94305
email: [email protected]
***********************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
Addison Engineering