Re: Rapid printing of high lines
1999-05-13
Angela Rasmussen
1999-05-13
Marc A. Unger
1999-05-14
Dirk De Bruyker
1999-05-13
Angela Rasmussen
1999-05-13
[email protected]
Re: Rapid printing of high lines
[email protected]
1999-05-13
Try a photoresist called SU-8. It can be patterned to >100 microns high with
great resolution.  Try electronic visions in Arizona to find out more about
the resist