Dear colleagues:

  I want to set up a XeF2 etching system (in its gaseous form not as a plasma)
for etching Silicon,
 but I wonder whether it reacts with the oil (used in vacuum pump) or not (I'm
worried about the
 formation of HF which can affect the future use of the chamber and pump)
  I also want to know what kind of valves I should use as the vacuums valve and
what is the best
 material for the chamber itself.
  Can anybody help me with these questions?

  Thanks in advance,
  Behraad Bahreyni


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
The Branford Group