Kevin A. Shaw
RE: why not use fluorine based chemistry to etch Al
Kevin A. Shaw
2000-05-10
Aluminum fluoride is not volatile a room temperature, Aluminum chloride is.

        -K

----------------------------
Kevin A. Shaw, Ph.D.
Senior Engineer
Kionix Inc.
22 Thornwood Dr.
Ithaca, NY 14850
Phone: (607) 257-1525, x125
Fax:   (607) 257-1612
Email: [email protected]

> -----Original Message-----
> From: Jay Mirza [mailto:[email protected]]
> Sent: Friday, May 05, 2000 1:14 PM
> To: [email protected]
> Subject: why not use flourine based chemistry to etch Al
>
>
> Hi guys,
>
> why chlorine based chemistry is preferred over lets say fluorine to etch
> Al in plasma etch (RIE type)?
>
> any help would be useful.
>
> thanks
>
> Jay Mirza
>
>


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Addison Engineering