MEMSnet Home: MEMS-Talk: Help Etching Silicon - Please?
Help Etching Silicon - Please?
2000-07-24
Argonide Nanomaterials
Help Etching Silicon - Please?
Argonide Nanomaterials
2000-07-24
This is a multi-part message in MIME format.
--------------883011E0BF1AC55C1F0A567F
Content-Type: text/plain; charset=us-ascii
Content-Transfer-Encoding: 7bit

Dear Colleagues,
Over time I've been a member of the group and have noticed how many
people come to the rescue for those in need of help. Well, now it's my
turn and I'm hoping someone out there can help me out with advice to any
or all questions.  Thanks in advance for your help.

Q1.  What is the preferred formulation for etching polycrystalline
silicon prior to metallization?
Q2.  What is the ratio of acid etchants (HF, nitric, acetic acid) for
removing the oxide from silicon?
Q3.  What are the preferred formulation for etchant for silicon dioxide?

Thanks again for the advice.

--------------883011E0BF1AC55C1F0A567F
Content-Type: text/x-vcard; charset=us-ascii;
 name="webmaster.vcf"
Content-Transfer-Encoding: 7bit
Content-Description: Card for Argonide Nanomaterials
Content-Disposition: attachment;
 filename="webmaster.vcf"

begin:vcard
n:Prorok;Cindi
tel;fax:(407) 322-1144
tel;work:(407) 322-2500
x-mozilla-html:FALSE
url:http://www.argonide.com
org:Argonide Nanomaterials Group
adr:;;;Sanford;FL;32771;USA
version:2.1
email;internet:[email protected]
title:Corporate Sales Div.
fn:Webmaster
end:vcard

--------------883011E0BF1AC55C1F0A567F--


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review