A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: 170 mikrometer thick glass wafers?
170 mikrometer thick glass wafers?
2000-08-09
Anders Olsson
170 mikrometer thick glass wafers?
Anders Olsson
2000-08-09
In one of our projects we have been using 4 inch Corning Pyrex 7740 wafers with
the thickness 170 micrometer. Unfortunately Corning can not deliver such thin
wafers to us anymore.

Does anyone have such wafers is stock they are willing to sell to us? We need
about 25 wafers.

Regards,
Dr. Anders Olsson
ACREO AB


reply