Hello all MEMS experts,

        We are doing poly1 beam bending of structures from MUMPs29 and
would like to find out the experimental gauge factor of the poly1 layer.
If you have seen this data published somewhere before please consider
letting us know. Thank you all very much.


-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-=-
            _______________________"oOo"____________________________
            Name:       Winston Sun ®]Ãý¦¨ (BSc 94, MSc 96)
            e-mail:     [email protected]
                        [email protected]
            URL:        http://www.acae.cuhk.edu.hk/~wsun
            phone:      (852)2609-8059 [Office] (852)2603-6002 [fax]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation
Addison Engineering