MEMSnet Home: MEMS-Talk: Is TMAH an isotropic etchant?
Is TMAH an isotropic etchant?
2000-12-28
Chang-Hwan Choi
Is TMAH an isotropic etchant?
Chang-Hwan Choi
2000-12-28
Hello, all?

I am making some microchannel. For channel etching,
someone recommended to use TMAH etchant as an
isotropic etchant for Silicon instead of DRIE dry
etching which is my preferred method. But, as far as I
know, TMAH is an anisotropic etchant of Silicon
similar to KOH. What I know as the isotropic etchant
of Silicon is HNA(HNO3+H2O+NH4F). Can the TMAH be
isotropic? And can photoresist be a mask for TMAH and
HNA wet etching?

Thank you and have a happy new year.

Chang.


=====
Chang-Hwan Choi
Brown University
Division of Engineering, Box D
Providence, RI 02912, U.S.A.

Tel: (401)867-6017(H), (401)863-2656(O), Fax: (401)863-9028
Email: [email protected], [email protected]

__________________________________________________
Do You Yahoo!?
Yahoo! Photos - Share your holiday photos online!
http://photos.yahoo.com/


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review