I am performing some cutting edge lithography on aluminum oxide. I am
fabricating features down to 4 microns in copper with aspect ratios of >4:1.
The process is not too expensive. Right now I am working on 4"x4" ceramic. I
believe that it can be scaled up to larger surfaces, even on polymeric
substrates. Are there any obvious industrial applications (and end
users)that I ought be pursuing? Or, are there fabricators that I ought be
pursuing joint venture with? Please be as specific as possible. I already
realize that people have chatted about: "Oh boy PCB people would love it!".

Thank you,

Jim Intrater
President
Integer Engineering Corp.
[email protected]


-----------------------------------------------
FREE! The World's Best Email Address @email.com
Reserve your name now at http://www.email.com


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Addison Engineering
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation