MEMSnet Home: MEMS-Talk: Sputtering gold on POM (Poly-oxy-methylene)
Sputtering gold on POM (Poly-oxy-methylene)
2001-06-15
Steve Lai Foo Khuen
Sputtering gold on POM (Poly-oxy-methylene)
Steve Lai Foo Khuen
2001-06-15
Hello there,
Could anyone help me ?
I need to sputter gold onto POM but somehow there's no adhesion to the POM.
The POM could not be etched ( using Ar gas)  and i'm running out of ideas.
I was advised to sputter an adhesion layer before sputtering gold but the
problem may be the same, no adhesion to the POM surface.

Thanks for the help in advance
Steve


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics