Dear all,
We are experiencing problems with high electrical resistivity of Cr/Au thin
films.
The films consist of 0.03um Cr and 0.3um Au, deposited by ion beam
sputtering, with no subsequent heat treatment.

The resitivity we achieve is ~x7 that of bulk gold, we know that 
reply