Dear Inna,

Thanks for your interest in PMGI....Microchem Corp is the manufacturer
of the aforementioned Resist, I would be pleased to share information
with you .... Please feel free to contact me at [email protected] or
by telephone on 617-965-5511 xt 308...

Best regards

Mark Shaw
Product Development & Applications Manager
MicroChem Corp.

-----Original Message-----
From: [email protected]
[mailto:[email protected]]
Sent: Tuesday, September 11, 2001 12:01 PM
To: [email protected]
Subject: mems-talk digest, Vol 1 #42 - 7 msgs


Send mems-talk mailing list submissions to
        [email protected]

To subscribe or unsubscribe via the World Wide Web, visit
        http://fab.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
        [email protected]

You can reach the person managing the list at
        [email protected]

When replying, please edit your Subject line so it is more specific
than "Re: Contents of mems-talk digest..."


Today's Topics:

   1. PMGI (Inna Mushkatinskaya)
   2. RE: Hot Embossing Mould Insert (Luesebrink Helge)
   3. companies that do wafer bonding in San Diego? (Felix Lu)
   4. Acoustic impedance ([email protected])
   5. Looking for used MEMS equipment (Andy Beregszaszi)
   6. Optical Property of SiC (Jiangang Du(John Duke))
   7. about etching glass (xuyutao)

--__--__--

Message: 1
Date: Mon, 10 Sep 2001 16:42:30 -0400
From: Inna Mushkatinskaya 
Reply-To: [email protected]
Organization: Anvik Corporation
To: [email protected]
Subject: [mems-talk] PMGI

This is a multi-part message in MIME format.
--------------E9B0562FA76C3533982D0F7E
Content-Type: text/plain; charset=us-ascii; x-mac-type="54455854";
x-mac-creator="4D4F5353"
Content-Transfer-Encoding: 7bit


Hello,

I'm looking for any information on PMGI. I'm using it as a photo resist
at 248
nm. Does anybody have experience with photolithography use of PMGI. I
have lots
of questions and will appreciate if somebody shares any information with
me.

Thanks a lot,

Inna.

--------------E9B0562FA76C3533982D0F7E
Content-Type: text/x-vcard; charset=us-ascii;
 name="innam.vcf"
Content-Transfer-Encoding: 7bit
Content-Description: Card for Inna Mushkatinskaya
Content-Disposition: attachment;
 filename="innam.vcf"

begin:vcard
n: Mushkatinskaya;Inna
tel;fax:914-345-2452
tel;work:914-345-2442
x-mozilla-html:FALSE
url:www.anvik.com
org:Anvik Corporation
adr:;;6 Skyline Drive;Hawthorne;NY;10532;USA
version:2.1
email;internet:[email protected]
title:Senior Process Specialist
x-mozilla-cpt:;1
fn:Inna  Mushkatinskaya
end:vcard

--------------E9B0562FA76C3533982D0F7E--




--__--__--

Message: 2
From: Luesebrink Helge 
To: [email protected], "'[email protected]'" 
Subject: RE: [mems-talk] Hot Embossing Mould Insert
Date: Mon, 10 Sep 2001 17:25:34 -0400

Emer,

The most frequently used techniques are


CNC (Computerized Numerical Control):
Large Features, Stainless Steel, Robust
DEEMO (Dry-Etch Electroplate Mold):
Medium Features, Nickel, Robust
LIGA (LIthography, Galvanoformung, Abformung):
Small Features, Nickel, Short Life
Silicon Etch (Dry Etch, Wet Chemical Etch):
Medium Features, Silicon, Short Life

Best regards,
Helge






                -----Original Message-----
                From:   Emer O'Reilly [mailto:[email protected]]
                Sent:   Friday, August 31, 2001 6:52 AM
                To:     '[email protected]'
                Subject:        [mems-talk] Hot Embossing Mould Insert

                Hi all.

                I am researching different possibilities to make a mould
insert for our hot
                embosser. Apart from the LIGA technique and etching of
silicon, has anyone
                any experience of other ways and materials?

                Thanks

                Emer



                _______________________________________________
                mems-talk mailing list
                [email protected]
                To unsubscribe or change your list options, use:
                 http://fab.mems-exchange.org/mailman/listinfo/mems-talk


--__--__--

Message: 3
From: Felix Lu 
To: [email protected]
Date: Mon, 10 Sep 2001 15:59:41 -0700 (PDT)
Subject: [mems-talk] companies that do wafer bonding in San Diego?

Hi,

   does anyone know of any companies who deal with wafer bonding in the
San Diego area? thanks.

Felix Lu
[email protected]


--__--__--

Message: 4
Date: Mon, 10 Sep 2001 17:58:55 -0700 (MST)
From: [email protected]
To: [email protected]
Subject: [mems-talk] Acoustic impedance

Hi,
I would be grateful if anybody could give me the acoustic impedence for
the
following materials
AlNOx,SiO2,Tungsten (w) and AlN.
I would also like to know a reference book that would give me the
acoustic
impedence of materials in general.
Thank you,
Regards,
Sushant

Sushant Salgar
Research Assistant,
Center for Solid State Electronics Research,
Electrical Engineering Dept,
Arizona State University.



--__--__--

Message: 5
From: Andy Beregszaszi 
To: [email protected]
Date: Mon, 10 Sep 2001 21:08:36 -0400
Subject: [mems-talk] Looking for used MEMS equipment

Hello all,

I'm looking to purchase a used RIE (preferrably a March CS 1701), a gas
cabinet, and cleanroom equipment.  If anyone knows where I may find this
stuff, I'd appreciate it.

Andy Beregszaszi
Graduate Student
Florida International University
Dept. of Mechanical Engineering



--__--__--

Message: 6
Date: Mon, 10 Sep 2001 22:48:29 -0400
From: "Jiangang Du(John Duke)" 
To: "[email protected]" 
Subject: [mems-talk] Optical Property of SiC

Anyone can recommend me a resource of optical property for SiC,such like
transparancy,reflection,diffraction coefficient,etc.
Since SiC has so many poly forms, a complete list of its optical
property in various forms is preferred.
--
Regards,
*************************************************
John Duke
**************************************************


--__--__--

Message: 7
Date: Mon, 10 Sep 2001 21:31:12 -0600
To: [email protected]
From: xuyutao 
Subject: [mems-talk] about etching glass

I wanted to etch cover glass up to 50um using Buffed HF with Shipley PR
1818 as an etching mask. However, the photoresist was stripped after 10
min
etching. Also the etching rate is only 500 angstrom /min. So could
someone
tell me how to solve the etching mask problem and also introduce me a
faster etchant? Thanks

Tao YU
ECE Department
Colostate State University




--__--__--

_______________________________________________
mems-talk mailing list
[email protected]
http://fab.mems-exchange.org/mailman/listinfo/mems-talk


End of mems-talk Digest


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing