Anodic Bond to Metal
2001-10-01
Roger Shile
Anodic Bond to Metal
Roger Shile
2001-10-01
Can someone suggest a metal that can be anodically bonded to Pyrex and won't
be etched by KOH?

I understand that aluminum bonds well to Pyrex, but I'm afraid, my subsequent
KOH etch will be a problem.

Someone on this forum stated that Cr is not attacked by KOH, however I don't
seem to be able to anodically bond Pyrex to Cr.

reply