> Date: Thu, 30 May 1996 11:59:01 -0400 (EDT)
> From: Michael Hershey 
> Subject: RIE services
> To: [email protected]
> Does anyone know where I could go to get Reactive Ion Etching (RIE)
> work done (to remove silicon and silicon oxide) on a few wafers?
> I understand Berkely may provide this service.
The University of California at Berkeley - Microfabrication Laboratory
(Microlab) equipment capabilities can be found in our www sight: http://
argon.eecs.berkeley.edu:8080/Microlab.html

Process related inquries should be directed to: John Knudsen, Process
Supervisor: [email protected]

We have several etchers. Our standard cmos etchers consist of 4 Lams:
Lam 490 nitride
Lam 580 oxide
Rainbow 6400 poly
Lam 690 aluminum

The Rainbow 6400 is the only Lam etcher capable of RIE. We do not currently
operate the Rainbow in the RIE mode.

Sincerely,
Bob Hamilton
Maint. Sup.
o


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics