MEMSnet Home: MEMS-Talk: Fabrication of micro structure based on PMMA
Fabrication of micro structure based on PMMA
2001-11-03
Wong Tak Sing
2001-11-05
reinhardt
Fabrication of micro structure based on PMMA
reinhardt
2001-11-05
www.microtec-d.de may have a solution for your product, please
email further details to [email protected]

Best regards
Andrea
----- Original Message -----
From: "Wong Tak Sing" 
To: 
Sent: Saturday, November 03, 2001 6:23 AM
Subject: [mems-talk] Fabrication of micro structure based on PMMA


> Hi MEMS people,
>
>   I would like to ask whether there are ways to make a micro structure
(depth:200um, length:10mm, width:5mm) on the PMMA substrate.  The micro
strucure is made of PMMA.  Could anyone suggest me the way how to fabricate
the structure (by etching, laser cutting etc.)?
>
>   Thank you in advance!
>
> Victor
> Student Researcher
> Center for Micro and Nano Systems
> The Chinese University of Hong Kong
>
>
>
>
> ________________________________________________________________
> Sent via the WebMail system at sciencescholars.net
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group