MEMSnet Home: MEMS-Talk: Thick SU8 Problems
Thick SU8 Problems
2001-11-12
Kevin Banks
Thick SU8 Problems
Kevin Banks
2001-11-12
Hi,
I'm working on research with SU8-100 at the University of Dundee, Scotland.
I've succeeded in attaining re-producable films of SU8 >400um on a silicon
substrate. However, after UV exposure, as soon as I begin the post exposure
bake, I get heavy deformations (ripples) in the
film surface. I've tried everything I can think of to stop this, including
starting from room temp, but to no avail. Can anybody suggest something????
Thanks in advance for your help.

Kevin Banks

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer