On Thu, 13 Jun 1996, Kevin M. Walsh wrote:
> Mike,
>
> Would you mind sharing your findings on RIE services available.  Sources
> and cost specifically.
>
> Thanks,
> Kevin Walsh
>
> --
> Dr. Kevin M. Walsh
> Electrical Engineering Department, Speed Scientific School
> University of Louisville, Louisville, KY 40292
> (502) 852-0826
>
> Internet address: [email protected]
>
>
Kevin,

Happy to do so (see below). For cost, it's probably best to contact them with
your specific requirements.

Mike Hershey

RIE Service Providers

#1 National Optics Institute

Tim Pope
    tel: 418-657-7006
    e-mail: [email protected]

#2 University of California

Bob Hamilton
    Maint. Sup.
    tel: 510-642-2716
    e-mail: [email protected]

#3 University of Minnesota

Dr. Greg Cibuzar
    Manager, Microtechnology Laboratory
    (612) 625-8079
    (612) 625-5012 fax
    e-mail: [email protected]
    Microtechnology Laboratory WWW site: http://www.ee.umn.edu/groups/mtl/

#4 MCNC

Dr. Mark D. Walters
    Program Manager
    MEMS Technology Applications Center
    MCNC, PO BOX 12889, Research Triangle Park, NC 27709-2889
    Phone: (919) 248-1864
    Fax: (919) 248-1455
    email: [email protected]
    URL: http://mems.mcnc.org

#5 Microelectronics Research Center at NJIT

Prof. Durga Misra
    tel: 201-596-5739

#6 Case Western Reserve University

Jeff Melzak
    Lab Manager
    tel: 216-368-3628
    e-mail: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group