MEMSnet Home: MEMS-Talk: SU-8 'T-topping' problem and solution using i-line filter
SU-8 'T-topping' problem and solution using i-line filter
2001-12-04
N. Farrington
SU-8 'T-topping' problem and solution using i-line filter
N. Farrington
2001-12-04
Hi there,

I have been using various formulations of SU-8 which has been
made in house (although commercial mixes have also been used).
Unfortunately the structures have been suffering from an
exaggerated negative sloping sidewall problem commonly referred
to as 'T-topping'.  The latest base processing guidelines on the
MCC website blame this problem on the lower wavelength (313nm
and 334nm) output lines of mercury vapour lamps and suggest that
the problem can be eliminated by optimising the spectral
bandwidth (ie using an i-line filter).

I was just wondering if anyone had experienced this problem
and taken this step to solved the problem.

Thanks in advance,

Novak Farrington
_____________________________________

Novak Farrington
Institute of Microwaves and Photonics
School of Electronic and Electrical Engineering
University of Leeds
Leeds LS2 9JT
UK

Tel. +44 (0)113 233 2092
Fax. +44 (0)113 233 2032
email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
MEMStaff Inc.
Process Variations in Microsystems Manufacturing