try two quartz (fused silica) photomasks with the chrome stripped off.

shay

[email protected] wrote:

> Sir/Madam,
>          In the abscense of a proper bonding equipment; Can anyone tell
> me , "How two wafers can be held together in a furnace/oven", to perform
> a "Direct bonding process".
>    To be more precise, what kind of fixture materials can be used for
> temperatures in the range of 1000 deg.C.  If anyone knows any company that
> provides these kind of fixtures , please forward the information.
>
> Regards,
> javeed shaikh mohammed.
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Addison Engineering
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing