MEMSnet Home: MEMS-Talk: Ag Etching
Ag Etching
2001-12-19
Rivas, Isabel
2001-12-19
Qingwei Mo
Ag Etching
Rivas, Isabel
2001-12-19
Hi,

I'm looking for an etchant able to remove an Ag thin film that has been
sputtered on a soda lime glass.

The glass surface must remain undamaged after the etching process.

Best regards,

Isabel Rivas Guerrero
E-mail: [email protected] 
CEIT, Seccisn de Microelectrsnica.
Paseo de Manuel Lardizabal, 15.
20018 San Sebastian, Spain
Tel.: (34) 943 212 800
Fax.: (34) 943 213 076

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics