Making 0.15um thick SiO2 film by anodic oxidation.
2002-01-07
Fan Frank
Making 0.15um thick SiO2 film by anodic oxidation.
Fan Frank
2002-01-07
Dear MEMS-Talk member:

I'm a graduate student and I have some research problem to consult with
you.

Now I want to make thick SiO2 film on n-type (100) silicon under normal
temperature by anodic oxidation method. The thickness is about 0.15um. Do
you think it's feasible?  If it's feasible, can you tell me under which
conditions such as concentration of HCl, voltage, illumination, time, I can
get such a thickness?

Thank you very much!
Fan Xinyu
January 7th,2002




_________________________________________________________________
SkA*;z5DEsSQ=xPP=;Aw#,GkJ9SC MSN Messenger#:
http://messenger.microsoft.com/cn

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMS Technology Review
Mentor Graphics Corporation