Hi all,
i wanted to once again ask u about the Porous silicon bcz i still have some
problems as i got some info about it but i donot understand  how the current
field lines will be in the BULksilicon and Porous silicon and how will they
change with time.

i will also like to ask if there is anz software that can simulate or show
how the current lines will go in the Electrolyte solution and the Interface
and the silicon both Porous silicon and bulk si.
i wanted to search for some info about these simulators which can show the
electric filed or
current lines in a solution but i ended up with nothing.
please give some ideas in this direction.
thanx
Fahad Ashfaq
germany

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
University Wafer