MEMSnet Home: MEMS-Talk: Rectangular wafer cassettes
Rectangular wafer cassettes
2002-02-04
Eric Lagally
2002-02-05
Klauder, Jr., Philip R.
2002-02-05
Mac McReynolds
2002-02-05
Roger Brennan
2002-02-07
Liz Shelley
2002-02-08
Roger Brennan
Rectangular wafer cassettes
Mac McReynolds
2002-02-05
Integris bought out Fluoroware, and, to the best of my knowledge, now
carries the full line of teflon and plastic boxes, carriers, etch baskets,
etc.  At least, that's where I buy them.

Mac McReynolds
R&D Manager
Caliper Technologies Corp.
605 Fairchild Drive
Mountain View, CA 94043-2234
Tel:  650-623-0710
Fax:  650-623-0521

> ----------
> From:         Eric Lagally
> Reply To:     [email protected]
> Sent:         Monday, February 4, 2002 3:34 PM
> To:   [email protected]
> Subject:      [mems-talk] Rectangular wafer cassettes
>
> Hi,
>
>      We will be starting a project using rectangular
> glass slides (25 x 75 mm and 21 x 75 mm), and we are
> in need of ways to hold these slides for etching and
> cleaning processes (HF, Pirahna, etc.).  Does anybody
> know of a source for such things?  I know Entegris
> sells custom-sizable carriers, but they are designed
> for transport, and the materials they are made from
> (i.e., stainless steel) aren't good in etches.  Any
> help is appreciated.
>
>                          Eric
>
>
>
>
> =====
> Eric Lagally
> UCB/UCSF Joint Bioengineering Graduate Group
> Mathies Research Laboratory
> 313 Lewis Hall
> Berkeley, CA 94720
> Great stuff seeking new owners in Yahoo! Auctions!
> http://auctions.yahoo.com
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
The Branford Group
University Wafer