A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: the mechanical properties of p+ Silicon film
the mechanical properties of p+ Silicon film
2002-02-15
정옥찬
the mechanical properties of p+ Silicon film
정옥찬
2002-02-15
Hi
Does anybody know about the mechanical properties (Young's modulus, average
and gradient stress, and ultimate strength, ...) of a heavily boron doped
silicon film(t : 2-4 um) and some references about it?

Best regards,

Ok-Chan, Jeong




Ok-Chan, Jeong
School of Electronics Engineering
5 Wonchon-Dong, Paldal-Ku
Suwon-City,442-749, KOREA
Tel : +82-31-219-2488
Fax : +82-31-212-9531
PCS : 016-208-1288
http://www.ajou.ac.kr/~mems


=============================================================================
=
?l8. @NEM3], Daum http://www.daum.net
- DaumH8?x@; @'GQ @NEM3]
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Addison Engineering
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing