A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: black wax
black wax
2002-02-25
ABHIJAT GOYAL
2002-02-26
Maurice Norcott
2002-02-28
Dave Summers
2002-02-26
Karl Cazzini
2002-03-01
Roger Brennan
black wax
ABHIJAT GOYAL
2002-02-25
Hi,

 can you please suggest me some vendors for Black Wax as a mask for KOH etch.
Can you please tell me the vendors that are based in US only, since it will be
difficult for me to procure my order if they are outside the US.

  Also can you please suggest me something by which I can remove black wax after
I have etched.

Thanks in advance,

Abhijat Goyal


Abhijat Goyal
EE MEMS group,
MS candidate,
Dept. Of Electrical Engineering,
State College, PA

Ph: (R)814-2350917
    (O)814-8653664

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing