Lin Wang
Thin Wafer and PI etching
Lin Wang
1996-07-18
I'd like to get some 3", N(100), resistivity>5 Ohm-cm, 200um thick wafers.
Does anybody know where I can get them?  Besides, I want to etch polyimide
film the wafer, does anybody know the etchant for the polyimde wet etching?
Any reply will be appreciated. Thanks in advance,
Best regards,

Lin

**************************************************
Lin Wang,  Graduate Student
Department of Electrical and Computer Engineering
Beckman Institute, Rm B428C
University of Illinois at Urbana-Champaign
405 North Mathews Avenue
Urbana, IL 61801

e-mail: [email protected], [email protected]
Tel. (217)-333-1088(O), (217)-351-8976(R)
**************************************************


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMS Technology Review
Harrick Plasma, Inc.