EPI layer Etching
2002-03-05
aslam muhammad
2002-03-05
Kenneth Smith
2002-03-06
StéphaneDURAND
EPI layer Etching
aslam muhammad
2002-03-05
i have got silicon <100> wafers with EPI layer of Ar.
I want to etch through the silicon wafer to make some
windows but EPI works as etch stop(i think).  How can
I etch EPI layer with wet etchant like TMAH.  If i
keep on etching the wafer, EPI layer etches very
slowly but my mask ( SiO2 ) etches rapidly as compared
to EPI layer.  Is there any body to help, Please.

Thanks

M. Aslam
Try FREE Yahoo! Mail - the world's greatest free email!
http://mail.yahoo.com/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review