Hi Mathieu,

There's an article in Vacuum called "reactive ion etching of quartz and
silica-based glasses in CF4/CHF3 plasmas"
by Patrick W. Leech. Vacuum 55 (1999) pp. 191-196 (No info about mask
material though as far as I can see.)

and not about quartz but maybe informative:
Deep reactive ion etching of Pyrex glass using SF6 plasma, Sensors and
Actuators A: Physical, Volume 87, Issue 3, 5 January 2001, Pages 139-145


Kind regards,
Heiko van der Linden

*******************************
MESA+ Research Institute
      Twente University
         P.O. Box 217
     7500 AE Enschede
       The Netherlands
*******************************


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of BURRI Mathieu
Sent: Monday, March 11, 2002 12:17 PM
To: [email protected]
Subject: [mems-talk] DRIE of quartz


Dear MEMS society,

I want to make holes (diameter 3-5 um, depth 40-50 um) in a QUARTZ
substrate by DRIE etching. Which mask materials, photoresist,... should
be used? Any comments and/or etch recipes are welcome.

Thanks

Regards
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Addison Engineering
MEMStaff Inc.