2002-03-14
Paolo Bondavalli
2002-03-14
Liz Shelley
2002-03-14
RobDavis
2002-03-14
Bill Moffat
GLASS FRIT
RobDavis
2002-03-14
We have been working on that technology, we can change the differential
thermal expansion to match.  We are prototyping silicon carbide package or
surface mount board with a "quartz-like" glass frit.
Rob Davis
Scientist
Caldus Semiconductor
Richland Washington
1-509-375-4775

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Paolo Bondavalli
Sent: Thursday, March 14, 2002 7:59 AM
To: [email protected]
Subject: [mems-talk] GLASS FRIT


Dear Mems Experts
We are tried to use glas frit in order to realize hermetic packaging of
MEMS.
Could you give me more information about this technique?
The cure temperature, the principal suppliers, publications about it...
Thanks a lot
have a nice day.

*********************************************************
Dr. Paolo Bondavalli
R&D Engineer
LABCOM - Laboratoire Interconnexions Optiques et MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************************
Disclaimer: Opinions expressed herein are my own and may
  not represent those of my employer.
**********************************************************
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Harrick Plasma, Inc.
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing